Print this page

HW-9

Gas-Cooled Torch Family - 140 amp

Features

  • Compact body provides greater access to weld in confined or restricted areas.
  • Hard body provides superior heat and abrasion resistance for longest life.
  • Silicon rubber body provides improved resistance to breakage in rough duty.
  • Flexible head models provide added versatility for reaching hard-to-get-at applications.

Classifications

Specifications

HW-9
Capacity  
continuous-duty ac or dc with standard accessories 120 Amps
continuous-duty ac or dc with gas lens accessories 85 Amps
@ 50 % duty with standard or gas lens accessories 140 Amps
@ 75% duty ac with standard or gas lens accessories 100 Amps
Size  
Overall Length 6-7/8 in., 175 mm
Handle Diameter 3/4 in., 19 mm
Length of Head  
short cap 2-19/64 in., 58 mm
medium cap 3-9/32 in., 83 mm
long cap 7-5/16 in., 186 mm
Diameter of Head 3/4 in., 19 mm
Weight (less cable) 3.5 oz., 100 gm
Head Angle: HW9 70 degrees
Head Angle: HW9F Variable
Electrode Capacity 1/8 in.

Ordering

Configure this Model

Part No.

HW-9
Part No. Model / Product Description UPC
34561 HW-9/RV-2,12.5-FT S/A HW-20ARV 662067009534
37740 HW-9-2-121/2 S/A HW-20A 662067996919
37741 HW-9-2-25 S/A HW-20A 662067996926
19684 HW-9,70 DEG 12.5-FT S/A HW-20A 662067009701
19685 HW-9, 70 DEG 25-FT S/A HW-20A 662067009718
34562 HW-9/RV-2, 25-FT S/A HW-20ARV 662067009541
19922 HW-9F,FLEX 12.5-FT S/A HW20AF 662067009725
19923 HW-9F, FLEX 25-FT S/A HW-20AF 662067009732
19610 HW-9FV-12 TORCH 662067984145
19611 HW-9FV-25 TORCH 662067984152

Accessories

There are no accessories.

Extra Info

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.