| Wire Speed Range (*actual speed range will depend on the arc voltage) | 50 to 700 ipm, 1.3 to 17.8 m/min |
|---|---|
| Wire Diameter Capacity | 0.023 to 5/64 in., 0.8 to 2 mm |
| Primary Input (open circuit voltage or arc voltage) **not for use with AC power | |
| Minimum | 16 vdc |
| Maximum | 100 vdc, 113 v peak |
| Weight | 30 lbs., 13 kg |
| Physical Dimensions | |
| Width | 9.5 in., 241.3 mm |
| Height | 14.0 in., 355.6 mm |
| Length | 26.9 in., 683.3 mm |
| MobileMaster feeders will fit through | 16 in. diameter hole, 41 mm diameter hole |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 0558001334 | MOBILEMASTER IV NAS | 662067167951 |
| 0558001333 | MOBILEMASTER IV CC | 662067167944 |
| 0558001801 | MOBILEMASTER IV NAS W/METERS | 662067168668 |
| 0558001802 | MOBILEMASTER IV CC W/METERS | 662067168675 |
| Part No. | Model / Product Description |
|---|---|
| 37365 | KIT, FLOWMETER, M-MASTER, CO2 |
| 36658 | KIT, FLOWMETER, M-MASTER ARGON |
| 23540446 | KIT, DIGITAL METER SUITCASE |
| 36661 | KIT,BRNBK/GASFLOW,MOBILEMASTER |
| 36657 | Burnback Control Kit - Adjustable burnback stops the wire feed before the arc is stopped |
| 13735590 | CONTACTOR 1 POLE 12VDC 500ADC |
| 17511 | SPOOL ADAPTOR 8 |
| 34330 | SPOOL ADAPTOR 10 |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.