Portable solutions for professional TIG and Stick welding - two control panels available, both with all functions required for TIG DC, AC/DC and MMA welding.

| Mains voltage | 230/1 V/ph, 50/60 Hz |
|---|---|
| Fuse (slow) | 16 A |
| Maximum Output | 220/18.8 @ 20% duty cycle, TIG, A/V, 150/16 @ 60% duty cycle, TIG, A/V, 140/15.6 @ 100% duty cycle, TIG, A/V |
| Setting range TIG AC/DC | 3-220 A |
| Setting range MMA | 4-160 A |
| Open circuit voltage, V DC | 70 V |
| Power factor @ 100, TIG mode | .99 power |
| Efficiency @ 100%, TIG mode | 66% efficient |
| Enclosure class | IP 23 class |
| Dimensions (LxWxH) | 16.46 x 7.4 x 13.58 in., 418 x 188 x 345 mm |
| Weight | 33.07 lbs., 15 kg |
| CoolMini water cooling unit | |
| Cooling capacity, W | 700W/0.264 gpm at 104 degrees F, 700W/1 lpm at 40 degrees C |
| Coolant volume | 0.581 Gal., 2.2 l |
| Maximum flow | 0.528 g.p.m., 2.0 l.p.m. |
| Maximum pressure, 50/60 Hz | 33.4 p.s.i., 2.3 bar |
| Weight | 9.92/14.77 lbs., 4.5/6.7 kg |
| Dimensions (LxWxH) | 16.46 x 7.4 x 5.39 in, 418 x 188 x 137 mm |
| MMC Panels (* Hidden Functions) | |
| TA34 AC/DC | |
| MicroPulse* | 0.001-0.250 sec |
| Slope up | 0-10 sec |
| Slope down | 0-10 sec |
| Gas pre-flow* | 0-5 sec |
| Gas post-flow | 0-25 sec |
| Pulse, background time, DC | 0.01-2.5 sec |
| Frequency AC | 10-152 Hz |
| AC balance | 50-98 % |
| TA33 AC/DC | |
| Slope down | 0-10 sec |
| Gas pre-flow* | 0-5 sec |
| Gas post-flow | 0-25 sec |
| Frequency AC | 65 Hz |
| AC balance | 70 % |
| Plate thickness, DC | 0.004-0.287 in, 0.1-7.3 mm |
| Plate thickness, AC | 0.004-0.216 in, 0.1-5.5 mm |
| There are no accessories. |
|---|
Control Panels
Two control panel options are available – both with all functions required for TIG DC, AC/DC and MMA welding. The Caddy™ Tig TA34 AC/DC features an advanced control panel with Pulse TIG, AC Balance to control arc cleaning and penetration, AC Frequency to control arc width, and a special setting to control electrode preheating for better starts with a variety of electrodes. The control panel of the Caddy™ Tig TA33 simplifies AC and DC TIG welding. All you do is set the plate thickness, and the machine does the rest, making it easy to produce quality TIG welds.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.