Arcaloy 308/308H-16 was developed for welding types 304H and 347H stainless when high temperature service is required.
Arcaloy 308/308H-16 electrodes were designed for the welding Types 304H & 304 where temperature in excess of 700°F(375°C) requires additional creep strength. They can equally well be used for the welding of stainless steel Types 301, 302 and 305. In some cases where the creep ductility of 347 weld metal is a concern, Arcaloy 308/308H electrodes can be used. The basic-rutile thin coating of Arcaloy 308/308H-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking.
Operates on AC or DC current.
* This item is subject to Industry Alloy Surcharges

| Yield Stress | 66 ksi, 410 MPa |
|---|---|
| Tensile Strength | 89 ksi, 610 MPa |
| Elongation in 2" | 44 % |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.055 % |
| Mn | 1.7 % |
| Si | 0.45 % |
| Cr | 20 % |
| Ni | 10 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Ferrite | 6 FN |
| Diameter | Flat | Vertical | Overhead |
|---|---|---|---|
| 1/16 in., 1.6 mm | 20-35 Amps | 15-25 Amps | 20-30 Amps |
| 5/64 in., 2.0 mm | 30-50 Amps | 25-35 Amps | 30-40 Amps |
| 3/32 in., 2.4 mm | 40-70 (Plus 60-85) Amps | 35-50 (40-60) Amps | 40-60 Amps |
| 1/8 in., 3.2 mm | 65-100 (Plus 90-120) Amps | 55-70 (70-80) Amps | 60-85 Amps |
| 5/32 in., 4.0 mm | 100-145 (Plus 140-165) Amps | 85-100 (80-90) Amps | 95-120 Amps |
| 3/16 in., 4.8 mm | 130-190 (Plus 180-210) Amps | 100-115 Amps | 125-150 Amps |
| 1/4 in., 6.4 mm | 205-290 Amps |