Print this page

ARCALOY 308L-16

Arcaloy 308L-16 was developed for welding 304L stainless.

Features

Arcaloy 308L-16 electrodes were developed for the welding of Type 304L stainless steels but can be used for many other stainless steels including Types 301, 302 & 304. They are used extensively for the welding of chemical plant equipment and may be used successfully for the welding of Types 321 and 347 stainless steels provided the service temperature is less than about 700ºF(375ºC). The basic-rutile thin coating of Arcaloy 308L-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking.

Operates on AC or DC current.


* This item is subject to Industry Alloy Surcharges

Arcaloy 308L-16
  • Industry
  • Tank and Vessel Fabrication
  • Process
  • Shipbuilding
  • General Fabrication
  • Petrochemical
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.4; E308-16/E308L-16
    • CWB CSA W48 E308L-16
    • ASME IX F No. 5
    • ASME II SFA E308-16/E308L-16
    • QPL-22200/2; MIL-308L-16

Properties

Typical Properties
Yield Strength 66 ksi, 460 MPa
Tensile Strength 90 ksi, 520 MPa
Elongation in 2" 45 %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.7 %
Si 0.5 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.1 %
Ferrite 6 FN

SAW

Accessories

Depositions