ARCALOY 308L-17 Plus

Arcaloy 308L Plus electrode utilize a heavy coating to maximize performance in the flat and horizontal position.

Features

Arcaloy 308L-17 Plus electrodes have a heavy coating, produce a concave bead with minimum ripple and the slag is virtually self-cleaning. These electrodes are designed to weld Types 304, 304L, 321 and 347 for corrosion service at temperature up to about 600ºF(315ºC).
The excellent wetting action and very fine ripple minimize crevice corrosion and grinding time. This is particularly useful in the food and drink industry where a smooth polished surface is required.

* This item is subject to Industry Alloy Surcharges

Arcaloy Plus 308L-17
  • Industry
  • Rail Road Car
  • Process
  • General Fabrication
  • Food and Beverage
  • Shipbuilding
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.4; E308-17/E308L-17
    • ASME IX F No. 5
    • ASME II SFA 5.4 E308-17/E308L-17

Properties

Typical Properties
Tensile Strength 86 ksi, 550 - 620 MPa
Elongation in 2" 47 %
Typical Undiluted Weld Metal Analysis  
C 0.02 %
Mn 0.6 %
Si 0.8 %
Cr 19 %
Ni 10 %
Mo 0.1 %
Cu 0.1 %
Ferrite 6 FN