Print this page

ARCALOY 309/309H-16

Arcaloy 309/309H-16 is used for welding type 309 base metal when high temperature service is required. Usable on AC or DC current.

Features

Arcaloy 309/309H-16 is used for welding Type 309 base metal for all service temperatures designed for Type 309. Carbon content 0.04% minimum. It can be used for carbon and low alloy steels and stainless steel dissimilar joints.

* This item is subject to Industry Alloy Surcharges

Arcaloy 309/309H-16
  • Industry
  • Process
  • General Fabrication
  • Petrochemical
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ABS-AWS A5.4; E309-16
    • QPL MIL-E-22200/2 MIL-309-16
    • ASME II SFA E309-16
    • ASME IX F No. 5

Properties

Typical Properties
Yield Stress 55 ksi, 380 MPa
Tensile Strength 90 ksi, 620 MPa
Elongation in 2" 40 %
Typical Undiluted Weld Metal Analysis  
C 0.06 %
Mn 1.8 %
Si 0.5 %
Cr 24 %
Ni 13.5 %
Mo 0.1 %
Cu 0.1 %
Ferrite 7 FN

SAW

Accessories

Depositions

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps

Extra Info