ARCALOY 309MoL-15

Arcaloy 309MoL-15 is designed for applications requiring molybdenum with a standard 309L analysis. Ideal for cladding prior to joining stainless steel to low alloy steels. Best used out-of-position on DC current.

Features

Arcaloy 309MoL-15 is designed for applications requiring molybdenum with a standard 309L analysis. It is used primarily for welding Types 316L and 316 clad steels, or for the first layer of a molybdenum - bearing stainless steel cladding on mild or low alloy steels austenitic stainless steels - to carbon and low alloy steels, provided the service temperature is less than about 600ºF (316ºC). In the dissimilar joint, Arcaloy 309MoL can tolerate more dilution by carbon and low alloy steels than Arcaloy 309L-15. Post weld heat treatment should be given due consideration.

* This item is subject to Industry Alloy Surcharges

309MoL-15
  • Industry
  • Process
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.4; E309MoL-15/E309Mo-15
    • ASME IX F No. 5
    • ASME II SFA E309Mol-15/E309Mo-15

Properties

Typical Properties
Yield Stress 75 ksi, 510 MPa
Tensile Strength 95 ksi, 650 MPa
Elongation in 2" 39 %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.7 %
Si 0.6 %
Cr 22.7 %
Ni 13.4 %
Mo 2.3 %
Cu 0.1 %
Ferrite 16 FN

SAW

Accessories

Depositions

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps