Print this page

ARCALOY 316/316H-15

Arcaloy 316/316H-15 can be used in applications where 316 stainless needs improved due to higher service temperature. Best used out-of-position on DC current.

Features

Arcaloy 316/316H-15 can be used for welding Type 316 and should be used in applications where 316 or 316H stainless needs improved high temperature. In some cases, E16-8-2 electrodes should be used.

* This item is subject to Industry Alloy Surcharges

316/316H-15
  • Industry
  • Petrochemical
  • General Fabrication
  • Process
  • Steel Industry
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME II SFA E316-15/E316H-15
    • QPL-22200/2; MIL-316-15
    • ASME IX F No. 5
    • AWS A5.4; E316-15/E316H-15

Properties

Typical Properties
Yield Strength 66 ksi, 490 MPa
Tensile Strength 86 ksi, 590 MPa
Elongation in 2" 40 %
Typical Undiluted Weld Metal Analysis  
C 0.06 %
Mn 1.6 %
Si 0.4 %
Cr 19 %
Ni 11.5 %
Mo 2.3 %
Cu 0.2 %
Ferrite 6 FN

SAW

Accessories

Depositions

Extra Info