Arcaloy 316/316H-16 can be used in applications where 316 stainless needs improved due to higher service temperatures. Usable on AC or DC current.
Arcaloy 316/316H-16 should be used in applications where Type 316 stainless steel needs improved high temperature. In some cases an E16-8-2 filler metal should be used. It can also be used to weld Type 316 stainless steel for ambient temperature service.
* This item is subject to Industry Alloy Surcharges

| Yield Stress | 65 ksi, 490 MPa |
|---|---|
| Tensile Strength | 85 ksi, 660 MPa |
| Elongation in 2" | 40 % |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.05 % |
| Mn | 1.6 % |
| Si | 0.4 % |
| Cr | 19 % |
| Ni | 12 % |
| Mo | 2.3 % |
| Cu | 0.2 % |
| Ferrite | 5.5 FN |
| Diameter | Flat | Vertical | Overhead |
|---|---|---|---|
| 1/16 in., 1.6 mm | 20-35 Amps | 15-25 Amps | 20-30 Amps |
| 5/64 in., 2.0 mm | 30-50 Amps | 25-35 Amps | 30-40 Amps |
| 3/32 in., 2.4 mm | 40-70 (Plus 60-85) Amps | 35-50 (40-60) Amps | 40-60 Amps |
| 1/8 in., 3.2 mm | 65-100 (Plus 90-120) Amps | 55-70 (70-80) Amps | 60-85 Amps |
| 5/32 in., 4.0 mm | 100-145 (Plus 140-165) Amps | 85-100 (80-90) Amps | 95-120 Amps |
| 3/16 in., 4.8 mm | 130-190 (Plus 180-210) Amps | 100-115 Amps | 125-150 Amps |
| 1/4 in., 6.4 mm | 205-290 Amps |