Print this page

ARCALOY 316LF5-15

Arcaloy 316LF5-15 is an electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. Designed to weld type 316, 316L steels. Best used out-of-position on DC current.

Features

Arcaloy 316LF5-15 is similar to Arcaloy 316L except the chemistry is balanced to give a weld deposit with a minimum ferrite number of 5. Carbon content 0.04% maximum. It can be used to weld Type 304L stainless steel where the presence of molybdenum is not detrimental.

* This item is subject to Industry Alloy Surcharges

316LF5-15
  • Industry
  • Petrochemical
  • General Fabrication
  • Steel Industry
  • Process
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 5
    • AWS A5.4 E316-15/E316L-15
    • QPL-22200/2; MIL-316L-15
    • ASME II SFA E316-15/E316L-15

Properties

Typical Properties
Yield Strength 62 ksi, 430 MPa
Tensile Strength 81 ksi, 560 MPa
Elongation in 2" 40 %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.5 %
Si 0.5 %
Cr 19 %
Ni 12 %
Mo 2.4 %
Cu 0.2 %
Ferrite 6 FN