Print this page

ARCALOY 316LF5-16

Arcaloy 316LF5-16 is an electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. Designed to weld type 316, 316L steels. Usable on AC or DC current.

Features

Arcaloy 316LF5-16 is a E316L-16 electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. It can be used to weld Type 316L stainless steel where the presence of molybdenum is not detrimental.


* This item is subject to Industry Alloy Surcharges

316LF5-16
  • Industry
  • Process
  • Steel Industry
  • Petrochemical
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME II SFA E316-16/E316L-16
    • AWS A5.4 E316-16/E316L-16
    • QPL MIL-E-22200/2 MIL-316L-16
    • ASME IX F No. 5
    • Certified by CWB to CSA W48

Properties

Typical Properties
Yield Stress 65 ksi, 450 MPa
Tensile Strength 83 ksi, 570 MPa
Elongation in 2" 40 %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.5 %
Si 0.4 %
Cr 19 %
Ni 12 %
Mo 2.5 %
Cu 0.2 %
Ferrite 6 FN

SAW

Accessories

Depositions

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps

Extra Info