Arcaloy 316L-Plus electrode utilizes a heavy coating to maximize performance in the flat and horizontal position. Usable on AC or DC current.
Arcaloy 316L-17 Plus electrodes have a heavy coating and produce a concave bead with minimal ripple. The slag is virtually self-cleaning. Molybdenum increases the resistance to pitting corrosion caused by corrosive media such as sulfuric and sulfurous acids, sulphites, chlorides and cellulose solutions. For welding Types 316 & 316L stainless steels when bead appearance is important.
* This item is subject to Industry Alloy Surcharges

| Tensile Strength | 77 ksi, 535 MPa |
|---|---|
| Elongation in 2" | 45 % |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.02 % |
| Mn | 0.6 % |
| Si | 0.6 % |
| Cr | 19 % |
| Ni | 12 % |
| Mo | 2.5 % |
| Cu | 0.1 % |
| Ferrite | 7 FN |