Print this page

ARCALOY 317L-15

Arcaloy 317L-15 electrodes are recommended for welding type 317 and 317L. The addition of molybdenum improves the weld metal crack resistance. Best used out-of-position on DC current.

Features

Arcaloy 317L-15 electrodes are recommended for welding type 317 and 317L with a maximum 0.04% carbon in the weld deposit. The higher molybdenum content of these electrodes as compared to Arcaloy type 316L further reduces the susceptibility of pitting corrosion.

* This item is subject to Industry Alloy Surcharges

317L-15
  • Industry
  • General Fabrication
  • Petrochemical
  • Process
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 5
    • AWS A5.4; E317-15/E317L-15
    • QPL MIL-E-22200/2 MIL-317L-15
    • ASME II SFA E317-15/E317L-15

Properties

Typical Properties
Yield Strength 64 ksi, 440 MPa
Tensile Strength 84 ksi, 580 MPa
Elongation in 2" 40 %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.5 %
Si 0.5 %
Cr 19 %
Ni 13 %
Mo 3.5 %
Cu 0.3 %
Ferrite 8 FN

SAW

Accessories

Depositions

Extra Info