Print this page

Arcaloy ER308LSi

Arcaloy ER308LSi is a silicon enhanced MIG wire which significantly increases wetting action, resulting in a smooth weld to improve weldability and performance on 304 steels.

Features

Arcaloy ER308LSi is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18 Cr- 8% Ni type. The alloy has a low carbon content, making it particularly recommended where there is a risk of intergranular corrosion.

* This item is subject to Industry Alloy Surcharges

Arcaloy ER308LSi
  • Industry
  • Food and Beverage
  • Process
  • Automotive
  • General Fabrication
  • Welding Process
  • GMAW (MIG)
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER308Si/ER308LSi
    • ASME SFA 5.9 ER308Si/308LSi
    • Certified by CWB - AWS A5.9
    • ASME IX F No. 6

Properties

Typical Properties
GMAW using 98% Argon / 2% Oxygen  
Yield Stress 55 ksi, 380 MPa
Tensile Strength 85 ksi, 690 MPa
Elongation in 2" 40 %
Typical Chemical Analysis  
C 0.015 %
Mn 1.7 %
Si 0.8 %
S 0.01 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.2 %
Ferrite 10 FN

SAW

Accessories

Depositions

Short Circuit Transfer Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.030 in., 0.8 mm 156-312 ipm, 396-792 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 0.64-1.72 kg/hr
.035 in., 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg/hr
.045 in., 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg/hr