Arcaloy 310-16 electrodes were developed for the welding of type 310 stainless steel. Usable on AC or DC current.

Features

Arcaloy 310 electrodes were developed for the welding of type 310 stainless steel. Arcaloy 310 weld deposit exhibits the same chemical analysis and oxidation resistance as the base plate metal. It is considered standard practice to weld types 410, 430, and 502 with Arcaloy 310 or 309 where field welding is done and where it is not possible to preheat or anneal after welding.

* This item is subject to Industry Alloy Surcharges

Classifications

  • Classifications/Approvals

    • QPL 22200/2; MIL 310-16
    • ASME II SFA E310-16
    • ASME IX F No. 5
    • AWS A5.4; E310-16

Properties

Typical Properties
Yield Stress 65 ksi, 450 MPa
Tensile Strength 90 ksi, 610 MPa
Elongation in 2" 38 %
Typical Undiluted Weld Metal Analysis  
C 0.1 %
Mn 1.8 %
Si 0.5 %
Cr 26 %
Ni 21 %
Mo 0.1 %
Cu 0.1 %

SAW

Accessories

Depositions

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps