Print this page

ATOM ARC 8018-C1

Atom Arc 8018-C1 is an all-position low hydrogen electrode that deposits weld metal containing nominal 2.3% Ni in applications that require low temperature toughness.

Features

Atom Arc 8018-C1 electrodes deposit weld metal which contains nominal 2.33% Ni. Their principal use is in the welding of nickel-bearing steels for low temperature applications where toughness of the weld metal at low temperatures is important.

Atom Arc 8018-C1
  • Industry
  • Mobile Machinery
  • Process
  • Bridge Construction
  • Petrochemical
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.5; E8018-C1H4R
    • Certified by CWB to CSA W48
    • L.R.- 3m,3Ym(H15)
    • A.B.S.- 3Y
    • ASME SFA 5.5

Properties

Typical Properties
As Welded  
Yield Strength 80 ksi, 550 MPa
Tensile Strength 90 ksi, 620 MPa
Elongation in 2" 30 %
Stress Relieved 1 hr. @ 1150ºF (621ºC)  
Yield Strength 75 ksi, 515 MPa
Tensile Strength 86 ksi, 595 MPa
Reduction in Area 74 %
Elongation in 2" 30 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -75ºF (-59ºC)  
As Welded 47 ft.-lbs., 64 J
Stress Relieved 1 hr. @ 1150ºF (621ºC) 64 ft.-lbs., 87 J
Typical Undiluted Weld Metal Analysis  
C .04 %
Mn 1.1 %
Si .3 %
P 0.011 %
S 0.009 %
Ni 2.4 %

SAW

Accessories

Depositions

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 90 A 70 - 100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
1/8 in, 3.2 mm 120 A 90 - 160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
140 A 90 - 160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
5/32 in, 4.0 mm 140 A 130 - 220 3.1 lbs./hr., 1.4 kg./hr. 75 %
170 A 130 - 220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
3/16 in, 4.8 mm 200 A 200 - 300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
250 A 200 - 300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
7/32 in, 5.6 mm 250 A 250 - 350 6.5 lbs./hr., 2.9 kg./hr. 75 %
300 A 250 - 350 7.2 lbs./hr., 3.3 kg./hr. 74 %
1/4 in, 6.4 mm 300 A 300 - 400 7.7 lbs./hr., 3.5 kg./hr. 78 %
350 A 300 - 400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info

Preheat should be used on hardenable steels to prevent the formation of a hard heat-affected zone. Preheat may also be required in welding heavy sections.