Print this page

ATOM ARC 8018-W

Atom Arc 8018-W is an E8018-W2 all-position low hydrogen electrode designed for welding low-alloy, high-strength "weathering" steels.

Features

Atom Arc 8018-W electrodes are designed specifically for welding the low-alloy, high-strength "weathering" steels, such as ASTM A588, A242, Cor-Ten, and Mayari R®. The uniform color blend of weld deposit with "weathered" steel makes these electrodes an excellent choice when architectural appearance is important.

Atom Arc 8018-W
  • Industry
  • General Fabrication
  • Civil Construction
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.5; E8018-W2H4R
    • ASME SFA 5.5

Properties

Typical Properties
As Welded  
Yield Strength 83 ksi, 575 MPa
Tensile Strength 93 ksi, 640 MPa
Elongation in 2" 27 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0°F (-18°C)  
As Welded 90 ft.-lbs., 122 J
Typical Undiluted Weld Metal Analysis  
C .048 %
Mn 1.05 %
Si .50 %
P .012 %
S .009 %
Cr .57 %
Ni .56 %
Cu .52 %

SAW

Accessories

Depositions

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 90 A 70 - 100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
1/8 in, 3.2 mm 120 A 90 - 160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
140 A 90 - 160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
5/32 in, 4.0 mm 140 A 130 - 220 3.1 lbs./hr., 1.4 kg./hr. 75 %
170 A 130 - 220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
3/16 in, 4.8 mm 200 A 200 - 300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
250 A 200 - 300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
7/32 in, 5.6 mm 250 A 250 - 350 6.5 lbs./hr., 2.9 kg./hr. 75 %
300 A 250 - 350 7.2 lbs./hr., 3.3 kg./hr. 74 %
1/4 in, 6.4 mm 300 A 300 - 400 7.7 lbs./hr., 3.5 kg./hr. 78 %
350 A 300 - 400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info

Preheat should be used on hardenable steels to prevent the formation of a hard heat-affected zone. Preheat may also be required in welding heavy sections