Print this page

CORESHIELD 6

Coreshield 6 is an E70T-6 self-shielded flux-cored wire designed for flat and horizontal welds requiring Charpy V-notch properties. It is tested and certified to meet the new AWS A5.20 ‘D' designation requirements, making it an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Features

Coreshield 6 is a high productivity, high deposition gasless flux cored wire. This self-shielded wire is ideal for single or multiple pass weld applications in addition to providing high deposition rates, low spatter, and good penetration. Because of its stiffer weld puddle, Coreshield 6 offers exceptional multi-pass weld stacking characteristics, produces excellent bead appearance and X-ray quality weld deposits.

Coreshield 6 is run DCEP (electrode positive).

Please see Related Links on the right side of this page to download the Seismic Data Sheet and Seismic Certifications.

Coreshield 6
  • Industry
  • Shipbuilding
  • Bridge Construction
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • Seismic Certified "D"
    • SFA/AWS A5.20; E70T-6

Properties

Typical Properties
As Welded  
Yield Strength 67 ksi, 465 MPa
Tensile Strength 85 ksi, 590 MPa
Elongation in 2" 26 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC) 31 ft.-lbs., 42 J
Typical Undiluted Weld Metal Analysis  
C 0.12 %
Mn 0.8 %
Si 0.2 %
P 0.005 %
S 0.008 %
Ni 0.4 %
Al 0.7 %

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
5/64 in, 2.0 mm 275 A 22 150 ipm, 381 cm/min 6.4 lbs./hr., 2.9 kg./hr. 78.1 % 1 inches, 25.4 mm
325 A 23 200 ipm, 508 cm/min 8.5 lbs./hr., 3.8 kg./hr. 79.6 % 1 inches, 25.4 mm
390 A 24 300 ipm, 762 cm/min 12.2 lbs./hr., 5.5 kg./hr. 80.2 % 1 inches, 25.4 mm
475 A 27 400 ipm, 1016 cm/min 16.3 lbs./hr., 7.3 kg./hr. 80.3 % 1 inches, 25.4 mm
535 A 29 500 ipm, 1270 cm/min 20.7 lbs./hr., 9.3 kg./hr. 81.2 % 1 inches, 25.4 mm
600 A 31 600 ipm, 1524 cm/min 25.7 lbs./hr., 11.5 kg./hr. 81.7 % 1 inches, 25.4 mm
3/32 in, 2.4 mm 265 A 22 100 ipm, 254 cm/min 6.1 lbs./hr., 2.9 kg./hr. 78.7 % 1 inches, 25.4 mm
365 A 23 150 ipm, 381 cm/min 9.3 lbs./hr., 4.2 kg./hr. 79.8 % 1 inches, 25.4 mm
415 A 23 200 ipm, 508 cm/min 12.5 lbs./hr., 5.6 kg./hr. 80.9 % 1 inches, 25.4 mm
530 A 26 300 ipm, 762 cm/min 19.0 lbs./hr., 8.5 kg./hr. 81.8 % 1 inches, 25.4 mm
615 A 29 400 ipm, 1016 cm/min 25.8 lbs./hr., 11.6 kg./hr. 81.8 % 1 inches, 25.4 mm