CORESHIELD 10

Coreshield 10 is a self-shielded flux cored welding wire designed for high speed single pass welding of thin gauge carbon, aluminized and galvanized steels.

Features

Coreshield 10 is a self-shielded flux cored welding wire designed for high speed single pass welding of thin gauge carbon, aluminized and galvanized steels. Its low spatter and excellent bead appearance makes it an ideal choice for high production applications. The use of DCEN (electrode negative) minimizes the risk of burn-through. High deposition efficiencies make it an ideal choice for automation. Coreshield 10 produces good wetting characteristics at high speeds making it suitable for robotic applications. It is designed to be used on automotive components, semi-trailer frames and axles, hot water tanks and door frames.

Coreshield 10
  • Industry
  • General Fabrication
  • Automotive
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20; E70T-14
    • ASME SFA 5.20

Properties

Typical Properties
As Welded  
Transverse Tensile Strength 92 ksi, 635 MPa
Longitudinal Guided Bend Test Satisfactory
Typical Undiluted Weld Metal Analysis  
C 0.05 %
Mn 1.4 %
Si 0.3 %
P 0.015 %
S 0.02 %
Al 1.0 %
Ti 1.0 %

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.045 in, 1.2 mm 80 A A 13 60 ipm, 152 cm/min 1.1 lbs./hr., .50 kg./hr. 76 % 1/2 inches, 12.7 mm
150 A A 17 118 ipm, 300 cm/min 2.6 lbs./hr., 1.18 kg./hr. 88 % 1/2 inches, 12.7 mm
225 A A 18 226 ipm, 574 cm/min 5.1 lbs./hr., 2.31 kg./hr. 90 % 1/2 inches, 12.7 mm
1/16 in, 1.6 mm 175 A A 14 61 ipm, 155 cm/min 2.1 lbs./hr., .95 kg./hr. 73 % 1/2 inches, 12.7 mm
220 A A 18 78 ipm, 198 cm/min 3.3 lbs./hr., 1.50 kg./hr. 83 % 1/2 inches, 12.7 mm
275 A A 19 108 ipm, 274 cm/min 4.8 lbs./hr., 2.18 kg./hr. 93 % 1/2 inches, 12.7 mm
5/64 in, 2.0 mm 250 A A 20 58 ipm, 147 cm/min 4.0 lbs./hr., 1.81 kg./hr. 94 % 3/4 inches, 19.1 mm
300 A A 21 85 ipm, 216 cm/min 5.1 lbs./hr., 2.31 kg./hr. 85 % 3/4 inches, 19.1 mm
400 A A 27 143 ipm, 363 cm/min 9.2 lbs./hr., 4.17 kg./hr. 90 % 3/4 inches, 19.1 mm

Extra Info

Procedure

  • Coreshield 10 contains barium and fluoride compounds. It is unlikely that these limits may be reached before the general fume limit of 5 mg/m3 is reached. Consult MSDS for more information.