Print this page

CORESHIELD 15

Coreshield 15 is an all-position self-shielded flux cored welding wire for single pass applications. It produces smooth arc action, full slag coverage, easy slag removal and low spatter.

Features

Coreshield 15 is an all-position self-shielded flux cored welding wire for single pass applications. Coreshield 15 produces smooth arc action, full slag coverage, easy slag removal, and low spatter. The use of DCEN (electrode negative) current minimizes the risk of burn-through. Coreshield 15 is excellent for use on lap and fillet welds on thin gauge galvanized and mild steels in all welding positions. The availability of .030" (0.8 mm) diameter makes it possible to use this product on materials as thin as 18 gauge (1.22 mm). The wire is particularly suitable for thin gauge materials 0.030 - 3/16" (0.8-4.8 in.) in galvanised, zinc-aluminum carbon, or aluminised carbon steels. In structural fabrications, the product can be used where no seismic requirements are present.

Coreshield 15
  • Industry
  • Civil Construction
  • Automotive
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • SFA/AWS A5.20; E71T-14
    • SFA/AWS A5.20; E71T-GS

Properties

Typical Properties
As Welded  
Transverse Tensile Strength 89 ksi, 615 MPa
Longitudinal Guided Bend Test Satisfactory
Typical Undiluted Weld Metal Analysis  
C 0.23 %
Mn 0.7 %
Si 0.4 %
P 0.007 %
S 0.01 %
Al 2 %

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 80 A A 15 81 ipm, 206 cm/min .9 lbs./hr., .41 kg./hr. 75 % 3/8 inches, 9.5 mm
120 A A 17 155 ipm, 394 cm/min 1.7 lbs./hr., .77 kg./hr. 77 % 3/8 inches, 9.5 mm
200 A A 17 392 ipm, 995 cm/min 4.5 lbs./hr., 2.04 kg./hr. 81 % 3/8 inches, 9.5 mm
.045 in, 1.2 mm 95 A A 15 54 ipm, 137 cm/min .9 lbs./hr., .41 kg./hr. 74 % 1/2 inches, 12.7 mm
150 A A 17 118 ipm, 300 cm/min 2.1 lbs./hr., .95 kg./hr. 79 % 1/2 inches, 12.7 mm
225 A A 18 140 ipm, 356 cm/min 2.6 lbs./hr., 1.18 kg./hr. 82 % 1/2 inches, 12.7 mm
1/16 in, 1.6 mm 160 A A 17 56 ipm, 142 cm/min 2.1 lbs./hr., .95 kg./hr. 78 % 5/8 inches, 15.9 mm
200 A A 18 76 ipm, 193 cm/min 2.9 lbs./hr., 1.32 kg./hr. 80 % 5/8 inches, 15.9 mm
275 A A 19 132 ipm, 335 cm/min 5.2 lbs./hr., 2.35 kg./hr. 81 % 5/8 inches, 15.9 mm
5/64 in, 2.0 mm 185 A A 19 50 ipm, 127 cm/min 2.4 lbs./hr., 1.09 kg./hr. 77 % 1 inches, 25.4 mm
250 A A 20 91 ipm, 231 cm/min 4.5 lbs./hr., 2.04 kg./hr. 79 % 1 inches, 25.4 mm
300 A A 21 135 ipm, 343 cm/min 6.6 lbs./hr., 2.99 kg./hr. 81 % 1 inches, 25.4 mm

Extra Info

Procedure

Coreshield 15 contains barium and fluoride compounds. The limit for soluble barium may be reached before the general fume limit of 5 mg/m3 is reached. Consult MSDS for more information.