CORESHIELD 11-Ni3

Coreshield 11-Ni3 is an all-position self-shielded wire designed to produce weld metal with good toughness (minimum 20 ft-lbs at 0°F).

Features

Coreshield 11-Ni3 is an all-position self-shielded wire designed to produce weld metal with good toughness (minimum 20 ft-lbs at 0°F). In addition, Coreshield 11-Ni3 provides the good weldability of Coreshield 11. It features a smooth arc, low spatter, full slag coverage, and easy slag removal.
Coreshield 11-Ni3 is ideal for field welding of structural steel where impact toughness is specified. It can be used for single or multipass welding. Coreshield 11 is run DCEN.

Classifications

  • Classifications/Approvals

    • SFA/AWS A5.29; E81T11-Ni3

Properties

Typical Properties
As Welded  
Yield Strength 81 ksi, 560 MPa
Tensile Strength 91 ksi, 630 MPa
Elongation in 2" 24.5 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0°F (-18°C)  
As Welded 26 ft.-lbs., 35 J
Typical Undiluted Weld Metal Analysis  
C 0.04 %
Mn 0.26 %
Si 0.2 %
P 0.010 %
S 0.001 %
Ni 3.6 %
Al 1.6 %

SAW

Accessories

Depositions

Extra Info

Procedure

Coreshield 11-Ni3 contains fluoride and barium compounds. The limit for soluble barium may be reached before the general fume limit of 5 mg/m3 is reached. Fume extraction at the arc must be used if Coreshield 11-Ni3 is used indoors. Consult MSDS for more information.