Coreweld Ultra is a low fume, metal-cored wire with high deposition efficiency, excellent welder appeal and minimal clean up.
Coreweld 70 is a tubular wire containing ingredients primarily comprised of metal powder with additional arc stabilizers and alloying elements. The result is a high efficiency wire.
Coreweld C6 is a metal-cored wire designed to provide excellent arc characteristics, high travel speeds and minimal spatter.
Coreweld 80-D2 is a metal cored wire equivalent to ER80S-D2 solid wire.
Coreweld W is a metal cored wire designed for single or multipass welding on weathering grade steels.
Coreweld 80CNil is a metal cored wire designed for applications where good impact toughness is required.
This electrode has a high percentage of iron powder resulting in a high efficiency wire with only small islands of slag on the weld deposit.
Coreweld 110 is a metal cored electrode designed for single and multipass welding of high strength low alloy steels, such as T-1, HY-80, and HY-100.