COREWELD 80-D2

Coreweld 80-D2 is a metal cored wire equivalent to ER80S-D2 solid wire.

Features

Coreweld 80-D2 is a metal cored wire equivalent to ER80S-D2 solid wire. Coreweld 80-D2 produces higher deposition rates, better wetting action, with an absence of copper coating on the wire. Coreweld 80-D2 was developed for HSLA steels. This product is capable of single or multiple pass welding

Coreweld 80-D2
  • Industry
  • Process
  • General Fabrication
  • Automotive
  • Mobile Machinery
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • AWS A5.28; E80C-G
    • ASME SFA 5.28

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Yield Strength 77 ksi, 530 MPa
Tensile Strength 90 ksi, 620 MPa
Reduction in Area 62 %
Elongation in 2" 26 %
Stress Relieved 8 hrs. @ 1175ºF (635ºC) 75% Ar / 25% CO2 Gas  
Yield Strength 77 ksi, 530 MPa
Tensile Strength 90 ksi, 625 MPa
Reduction in Area 68 %
Elongation in 2" 26 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 75% Ar / 25% CO2 34 ft.-lbs., 46 J
Stress Relieved 8 hrs. @ 1175ºF (635ºC) CO2 25 ft.-lbs., 34 J
Testing Temperature -40ºF (-40ºC)  
As Welded 75% Ar / 25% CO2 23 ft.-lbs., 31 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.09 %
Mn 1.2 %
Si 0.3 %
P 0.010 %
S 0.018 %
Mo 0.4 %

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.035 in, 0.9 mm 150 A 25 V 320 ipm, 813 cm/min 4.4 lbs./hr., 1.2 kg./hr. 92 %
200 A 27 V 472 ipm, 1199 cm/min 6.5 lbs./hr., 2.95 kg./hr. 92 %
250 A 29 V 680 ipm, 1727 cm/min 9.4 lbs./hr., 4.26 kg./hr. 92 %
.045 in, 1.2 mm 250 A 28 V 330 ipm, 838 cm/min 8.0 lbs./hr., 3.63 kg./hr. 90 %
275 A 30 V 430 ipm, 1092 cm/min 11.1 lbs./hr., 5.03 kg./hr. 94 %
300 A 32 V 464 ipm, 1179 cm/min 11.6 lbs./hr., 5.26 kg./hr. 94 %
350 A 32 V 512 ipm, 1300 cm/min 12.7 lbs./hr., 5.76 kg./hr. 96 %
.052 in, 1.4 mm 275 A 29 V 262 ipm, 665 cm/min 8.0 lbs./hr., 3.63 kg./hr. 92 %
300 A 29 V 312 ipm, 792 cm/min 9.6 lbs./hr., 4.35 kg./hr. 93 %
325 A 30 V 328 ipm, 833 cm/min 10.1 lbs./hr., 4.58 kg./hr. 93 %
1/16 in, 1.6 mm 300 A 30 V 181 ipm, 460 cm/min 8.6 lbs./hr., 3.90 kg./hr. 89 %
350 A 30 V 241 ipm, 612 cm/min 11.9 lbs./hr., 5.40 kg./hr. 94 %
400 A 32 V 293 ipm, 744 cm/min 14.6 lbs./hr., 6.62 kg./hr. 94 %
450 A 34 V 333 ipm, 846 cm/min 16.2 lbs./hr., 7.35 kg./hr. 94 %
5/64 in, 2.0 mm 350 A 27 V 160 ipm, 406 cm/min 11.6 lbs./hr., 5.26 kg./hr. 94 %
400 A 28 V 185 ipm, 470 cm/min 13.2 lbs./hr., 5.99 kg./hr. 95 %
450 A 28 V 210 ipm, 533 cm/min 15.8 lbs./hr., 7.17 kg./hr. 97 %
500 A 29 V 280 ipm, 711 cm/min 20.4 lbs./hr., 9.25 kg./hr. 97 %
3/32 in, 2.4 mm 400 A 31 V 115 ipm, 292 cm/min 11.5 lbs./hr., 5.22 kg./hr. 95 %
450 A 31 V 138 ipm, 350 cm/min 14.5 lbs./hr., 6.58 kg./hr. 97 %
500 A 32 V 155 ipm, 394 cm/min 16.5 lbs./hr., 7.48 kg./hr. 97 %
550 A 32 V 197 ipm, 500 cm/min 21.0 lbs./hr., 9.53 kg./hr. 98 %

Extra Info

Shielding Gas

75% Ar / 25% CO2