Print this page

COREWELD 80C-Ni1

Coreweld 80CNil is a metal cored wire designed for applications where good impact toughness is required.

Features

Coreweld 80C-Ni1 is a metal cored wire for application where good low temperature impact toughness or weathering characteristics are required. It operates over a broad range of parameters, produces a smooth, spray transfer with minimal fume and spatter and is tolerant of light rust and millscale. The shielding gas used should be Ar 75-92% / 25-8% CO2.

Coreweld 80C-Ni1
  • Industry
  • General Fabrication
  • Process
  • Bridge Construction
  • Mobile Machinery
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • AWS A5.28; E80C-Ni1
    • CERTIFIED BY C.W.B.- AWS A5.28
    • ASME SFA 5.28

Properties

Typical Properties
As Welded 85% Ar / 15% CO2  
Yield Strength 70 ksi, 485 MPa
Tensile Strength 82 ksi, 565 MPa
Reduction in Area 66 %
Elongation in 2" 27 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded 75% Ar / 25% CO2 55 ft.-lbs., 75 J
Testing Temperature -50ºF (-46ºC)  
As Welded 85% Ar / 15% CO2 75 ft.-lbs.
Typical Undiluted Weld Metal Analysis  
85% Ar / 15% CO2  
C 0.04 %
Mn 1.5 %
Si 0.3 %
P 0.010 %
S 0.020 %
Ni 0.9 %

SAW

Accessories

Depositions

Extra Info

Shielding Gas

Ar 75-92% / 25-8% CO2