Dual Shield Arc 87 is a low slag/high deposition efficiency flux cored wire designed for joining heavy structural components.
Dual Shield Arc 70 is a large diameter flux cored wire for flat and horizontal welding over heavy rust and mill scale.
Dual Shield 111-AC is a flux cored wire for single or multipass operation on mild steel and on some low alloy steels.
Dual Shield 111A has low deoxidation potential, but good machineability.
Dual Shield 111-HD produces high deposition efficiency (86-90%).
Dual Shield 111-RB is a low slag, high deposition flux cored electrode designed for joining structural components made of low carbon steel. It is good over rust and primer.
Dual Shield Arc 90 is a low slag - high deposition efficiency flux cored wire designed for joining heavy structural steel components.
Dual Shield R-70 Ultra is a low fuming flux cored wire with a balanced chemistry .
Dual Shield SP is a flux cored single pass wire especially developed for welds of good contour and soundness regardless of the surface condition of the steel.
Dual Shield 110 has high deoxidation potential.
Dual Shield T-63 has high deoxidation potential. Single pass capability
Dual Shield Arc 71 is a all-position welding over moderate rust and mill scale. Spatter levels and fume generation rates are lower than comparable cored wires.
Dual Shield II 71 Ultra is an all-position flux-cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.
Dual Shield 7000 is the industry's first all position flux cored wire combines excellent performance features with the ability to produce high quality welds.
Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.
Dual Shield FC-717 is an all-position flux cored wire.
Dual Shield 7100 Ultra is an all-position wire with a uniquely balanced formulation to provide greater deposition and improved welding productivity.
Dual Shield 7100 LC is an all-position wire with a uniquely balanced chemistry to provide greater deposition and improved welding productivity.
Dual Shield T-62 is designed to weld mild and medium carbon steels using CO2.
Dual Shield II 70T-12H4 is an all-position, low hydrogen flux cored wire that provides excellent low temperature toughness. This flux cored wire provides a smooth arc and low spatter levels, excellent for construction, fabrication, offshore and railcar applications.
Dual Shield 70 Ultra Plus is an all-position wire that is uniquely designed to provide high deposition, outstanding all position performance and a fume emission rate approaching that of solid wires.
Dual Shield T-75 is a flux cored wire with a basic slag system designed for multiple pass welding and produces excellent properties in both the as welded and stress relieved conditions.
Dual Shield T-5 is a basic slag flux-cored wire that produces crack resistant, highly ductile weld deposits. It is especially produces recommended for medium to heavy fabrication, using a number of mild steels.
Dual Shield T-75H is a CO2 shielded, large diameter basic slag flux cored wire designed to provide weld deposits having excellent impact toughness and low diffusible hydrogen (less than 6 ml/100g). In addition, it provides a weld deposit that is highly resistant to solidification cracking, even in highly restrained joints.
Dual Shield II 70-LF is an extremely low fuming wire designed for use with 95% Ar - 5% CO2 shielding gas.
Dual Shield II 70T-12 is a mild steel flux cored wire with excellent mechanical properties.
Dual Shield 7000-A1 is an all-position wire recommended for 0.5% Mo steels.
Dual Shield 88-CM is a flux cored continuous wire depositing X-ray sound weld metal with a nominal analysis of 1.25% Cr, 0.5% Mo.
Dual Shield 8000-B2 is an all-position flux-cored wire containing 1% Cr - 0.5% Mo.
Dual Shield 8000-B2L is an all-position flux-cored wire for low carbon grades of 1. Cr - 0.5% Mo steels.
Dual Shield 98-CM is a Cr-Mo flux-cored wire designed to weld 2% Cr - 1% Mo steels.
Dual Shield 9000-B3 is an all-position flux-cored wire containing 2% Cr-1% Mo.
Dual Shield 9000-B3L is an all-position flux cored wire for low carbon grades of 2.25% Cr - 1% Mo steels.
Dual Shield B6 is an all position flux cored wire designed to weld Mo steels.
Dual Shield B9 is an all position flux-cored wire designed to weld 9% Cr -1% Mo(P91) steels.
Dual Shield II 80-NilH4 is an all position gas shielded flux-cored wire which that exhibits a smooth easily controlled arc and produces a spray-like transfer.
Dual Shield 88-C3 is a flux cored wire developed to deposit weld metal with impact toughness as low as -40ºF(-40ºC). The weld metal meets high X-ray standards for soundness.
Dual Shield 80-C3 is a flux cored wire designed for use with CO2 shielding. It deposits a nominally 1% Ni weld metal with impact toughness at temperatures as low as -20°F (-28°C). It features a stable arc and easily controlled weld puddle. The thin cover of slag is easily removed, even from deep grooves. Spatter levels are generally low. X-ray quality welds can easily be produced with Dual Shield 80-C3
Dual Shield 85-C1 is a basic slag multipass wire .
Dual Shield 8000-Ni2 is an all-position wire that deposits 2.5% Ni deposit with an 82 ksi (565 MPa) tensile strength.
Dual Shield 8100-Ni2 is an all-position wire that deposits a nominal 2.5% Ni with an 80 ksi(550 Mpa) tensile.
Dual Shield 9000-C1 is an all-position flux-cored wire which produces a 2.5% Ni deposit.
Dual Shield 150 is for high strength 1.5% Mn - 0.5% Mo steels.
Dual Shield II 100-D1 is an all-position flux cored welding wire specially formulated to weld quenched and tempered steels .
Dual Shield II 81-K2 is an all-position flux cored wire developed for low alloy high strength steels where low temperature impact toughness is required.
Dual Shield II 101-TM is an all-position flux cored wire developed to meet the stringent requirements of the military specification.
Dual Shield II 101-TC is an all-position wire developed to meet the U.S. Navy qualification tests for hydrogen levels of less than 0.05 ml/g of weld metal.
Dual Shield II 90-K2 is an all-position, high performance wire with low diffusible hydrogen levels.
Dual Shield 9000-M is an all-position Ni-Mo wire.
Dual Shield II 101H4M was developed to meet the stringent requirements of MIL-E-24403/2 and offshore welding, and it is an ideal choice for HSLA steels.
Dual Shield T-100 is a flux cored wire with excellent mechanical properties.
Dual Shield II 100 is an all-position wire that combines a high strength deposit with excellent impact toughness.
Dual Shield T-8 is a low alloy, high strength flux cored wire designed for welding of high strength quenched and tempered steels.
Dual Shield II 110 is an all-position flux cored wire which produces a smooth spray-like transfer, low spatter levels, easy slag removal and good arc direction.
Dual Shield T-115 is a basic slag flux cored wire designed for applications requiring a high strength weld deposit.
Dual Shield II 120M2 is a high strength, low alloy flux cored wire for welding HY-100 and HSLA-100 steels.
Dual Shield T-115-K3 is a basic, flux cored electrode designed to weld high strength steels up to 110 Ksi (760 MPa), using CO2 shielding gas. It provides good weld metal toughness and low diffusible hydrogen (less than 4 ml/100g).
Dual Shield T-125 is a basic, flux cored electrode designed to weld high strength steels up to 120 Ksi (830 MPa), using CO2 shielding gas.
Dual Shield T-95-M is a basic slag wire for HY-80 and other low alloy steels.
Dual Shield 8100-W is an all-position wire for weathering grade steels.
Dual Shield T-4130 is a flux cored wire with a specialized weld metal analysis designed for welding alloy steels.
Dual Shield T-4130-LN is a basic slag flux cored electrode designed to match the heat treating properties of such steels as SAE 4130 and 8630 when the Nickel analysis of less than 1% is required.