Print this page

DUAL SHIELD 111-HD

Dual Shield 111-HD produces high deposition efficiency (86-90%).

Features

Dual Shield 111-HD produces high deposition efficiency (86-90%). Use CO2 shielding gas.

DUAL SHIELD 111-HD
  • Industry
  • General Fabrication
  • Shipbuilding
  • Mobile Machinery
  • Civil Construction
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.20
    • AWS A5.20; E70T-1C

Properties

Typical Properties
As Welded  
Yield Strength 70 ksi, 485 MPa
Tensile Strength 81 ksi, 560 MPa
Reduction in Area 65 %
Elongation in 2" 28 %
Typical Undiluted Weld Metal Analysis  
C 0.06 %
Mn 1.03 %
Si 0.35 %
P 0.013 %
S 0.017 %

SAW

Accessories

Depositions

Extra Info

Shielding Gas

CO2