Dual Shield Arc 90 is a low slag - high deposition efficiency flux cored wire designed for joining heavy structural steel components.
Dual Shield Arc 90 is a low slag - high deposition efficiency flux cored wire designed for joining heavy structural steel components. It is for use in flat and horizontal position welding only. Dual Shield Arc 90 provides high deposition rates, high efficiency and excellent welding performance. Dual Shield Arc 90 weld beads have a thin slag cover that is easily removed. Fillet welds made with Dual Shield Arc 90 have a flat profile and good penetration.

| Typical Mechanical Properties | |
|---|---|
| Yield Strength | 70 ksi, 480 MPa |
| Tensile Strength | 82 ksi, 565 MPa |
| Elongation in 2" | 26 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature | |
| -20ºF (-29ºC) | 23 ft.-lbs., 31 J |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.05 % |
| Mn | 1.2 % |
| Si | 0.5 % |
| P | 0.009 % |
| S | 0.015 % |
CO2