Print this page

DUAL SHIELD R-70 Ultra

Dual Shield R-70 Ultra is a low-fuming, high-deposition E70T-9 flux cored wire. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Features

This flux cored welding wire produces smoother arc characteristics and lower welding fumes than many competitive flux cored wires. Dual Shield R-70 Ultra is also designed to have a greater tolerance of mill scale and surface oxides. The notch toughness in the as welded condition is also improved. Bead contour is flat to slightly convex and slag coverage is complete. Dual Shield R-70 Ultra wire is designed for flat/horizontal single or multi-pass applications on low or medium carbon steels using 100% CO2 shielding gas. Areas of application include railcar, heavy equipment, and general fabrication.

Please see Related Links on the right side of this page to download the Seismic Data Sheet and Seismic Certifications.

Dual Shield R-70 Ultra
  • Industry
  • General Fabrication
  • Civil Construction
  • Shipbuilding
  • Mobile Machinery
  • Rail Road Car
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • Seismic Certified "D"
    • AWS A5.20; E70T-1CH8/T-1M/T-9CH8/T-9M
    • QPL-24403/1; MIL-70T-1C
    • D.N.V.- II YMS(H15)
    • L.R.- 2S,2YS(H15)
    • A.B.S.- 2SA,2YSA
    • CERTIFIED BY C.W.B.- CSA W48
    • ASME SFA 5.20

Properties

Typical Properties
As Welded CO2  
Yield Strength 70 ksi, 485 MPa
Tensile Strength 82 ksi, 565 MPa
Reduction in Area 63 %
Elongation in 2" 26 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded CO2 28 ft.-lbs., 38 J
Testing Temperature -20ºF (-29ºC)  
As Welded CO2 25 ft.-lbs., 34 J
Typical Undiluted Weld Metal Analysis  
CO2  
C 0.02 %
Mn 1.4 %
Si 0.5 %
P 0.014 %
S 0.008 %

SAW

Accessories

Depositions

Extra Info

Shielding Gas

CO2