DUAL SHIELD II 71 Ultra

Dual Shield II 71 Ultra is an all-position flux-cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.

Features

Dual Shield II 71 Ultra is an all-position flux cored wire that displays exceptional impact properties when used with CO2. The improved properties qualify this wire to the Navy's "HY" classification. The "Ultra" series produces smoother arc characteristics and lower welding fumes. Dual Shield II 71 Ultra was developed to join low and medium carbon steel. The Military classification allows Dual Shield II 71 Ultra to be used for attaching steels of less than 80 ksi (552 MPa) yield to HY-80 and HY-100. Commercial applications include construction, shipbuilding, railcar, and heavy equipment industries. Weld metal analysis is similar to an E7018 low hydrogen electrode.

Dual Shield II 71 Ultra
  • Industry
  • Civil Construction
  • Shipbuilding
  • Bridge Construction
  • Rail Road Car
  • Mobile Machinery
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20;E71T-1CJ/T-12CJ
    • QPL-24403/1; MIL-71T-1C
    • QPL-24403/1; MIL-71T-1-HYC
    • D.N.V.- III YMS(H10)
    • G.L.- 3YH10S
    • L.R.- 3S,3YS(H10)
    • A.B.S.- 3SA,3YSA
    • CERTIFIED BY C.W.B.- CSA W48
    • ASME SFA 5.20

Properties

Typical Properties
As Welded  
Yield Strength 71 ksi, 495 MPa
Tensile Strength 79 ksi, 540 MPa
Reduction in Area 77 %
Elongation in 2" 28 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded 96 ft.-lbs., 130 J
Testing Temperature -20 F (-29 C)  
As Welded CO2 40 ft.-lbs, 54 J
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.4 %
Si 0.4 %
P 0.012 %
S 0.010 %