Dual Shield T-62

Dual Shield T-62 is designed to weld mild and medium carbon steels using CO2.

Features

Dual Shield T-62 is designed to weld mild and medium carbon steels using CO2. The steel should be reasonably clean and for greater efficiency weld horizontally. Mulitple pass horizontal fillets may be welding with Dual Shield T-62 without removing the slag from each weld bead.

Classifications

  • Classifications/Approvals

    • AWS A5.20; E70T-1C/T-1M/T-9C/T-9M

Properties

Typical Properties
As Welded CO2  
Yield Strength 74 ksi, 510 MPa
Tensile Strength 87 ksi, 600 MPa
Elongation in 2" 26 %
Reduction in Area 58 %
Typical Charpy V-Notch Inpact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded CO2 24 ft.-lbs., 33 J
Typical Undiluted Weld Metal Analysis  
As Welded CO2  
C 0.08 %
Mn 1.35 %
Si 0.55 %

SAW

Accessories

Depositions

Extra Info

Shielding Gas

CO2