DUAL SHIELD II 70T-12H4

Dual Shield II 70T-12H4 is an all-position, low hydrogen flux cored wire that provides excellent low temperature toughness. This flux cored wire provides a smooth arc and low spatter levels, excellent for construction, fabrication, offshore and railcar applications.

Features

Each of the new Dual Shield II H4 wires is an all-position flux cored wire that provides excellent low temperature toughness in both the as welded and/or stress relieved conditions (as applicable) when used with 75% Ar/25% CO2. Each can produce diffusible hydrogen levels of < 4mL/100g over a wide range of welding parameters. Dual Shield II 70T-12H4 also provides the smooth arc and low spatter levels characteristic of other Dual Shield II wires. Dual Shield II 70T-12H4 can be used in construction, heavy equipment fabrication, offshore oil components, shipbuilding, and railcar. Weld metal analysis is similar to E7018 & E7018-1 low hydrogen covered electrodes

Dual Shield II 70T-12H4
  • Industry
  • Mobile Machinery
  • Bridge Construction
  • Civil Construction
  • General Fabrication
  • Rail Road Car
  • Shipbuilding
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20; E71T-1MJH4/T-12MJH4
    • CERTIFIED BY C.W.B.- CSA W48
    • ASME SFA 5.20
    • D.N.V.- IV YMS(H5)
    • L.R.- 4Y40S(H10)
    • A.B.S.- 3SA,3YSA(H5)
    • G.L.- 4YH10S

Properties

Typical Properties
As Welded 75% Ar / 25% CO<sub>2</sub>  
Yield Strength 72 ksi, 495 MPa
Tensile Strength 80 ksi, 550 MPa
Reduction in Area 71 %
Elongation in 2" 27 %
Stress Relieved 2 hrs. @ 1150ºF (621ºC) 75% Ar / 25% CO2  
Yield Strength 68 ksi, 460 MPa
Tensile Strength 78 ksi, 540 MPa
Reduction in Area 73 %
Elongation in 2" 30 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 75% Ar / 25% CO2 79 ft.-lbs., 107 J
Stress Relieved 2 hrs. @ 1150ºF (621ºC) 75% Ar / 25% CO2 76 ft.-lbs., 103 J
Testing Temperature -40ºF (-40ºC)  
As Welded 75% Ar / 25% CO2 62 ft.-lbs., 84 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.027 %
Mn 1.08 %
Si 0.33 %
P 0.016 %
S 0.008 %