Dual Shield II 70-LF is an extremely low fuming wire designed for use with 95% Ar - 5% CO2 shielding gas.
Dual Shield II 70-LF is an extremely low fuming wire designed for use with 95% Ar - 5% CO2 shielding gas.

| Typical Mechanical Properties | |
|---|---|
| As Welded 98% Ar / 5% CO2 | |
| Yield Strength | 75 ksi, 515 MPa |
| Tensile Strength | 82 ksi, 565 MPa |
| Elongation in 2" | 27 % |
| Charpy V-Notch Toughness | |
| Testing Temperature @ -20ºF (-28ºC) | 60 ft.-lbs., 81 J |
| Typical All Weld Metal Analysis | |
| C | 0.04 % |
| Mn | 1.0 % |
| Si | 0.4 % |
| P | 0.012 % |
| S | 0.009 % |
| Ni | 0.4 % |
95% Ar / 5% CO2