Dual Shield 8100-W is an all-position wire for weathering grade steels.

Features

Dual Shield 8100-W is an all-position flux cored electrode developed specifically to color match with the low alloy, high strength weathering grade steels such as ASTM 588 & 242. Dual Shield 8100-W was designed for CO2 or Argon / CO2 shielding gas mixtures.

Dual Shield 8100-W
  • Industry
  • General Fabrication
  • Mobile Machinery
  • Rail Road Car
  • Automotive
  • Bridge Construction
  • Shipbuilding
  • Civil Construction
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • CERTIFIED BY C.W.B.-AWS A5.29; E81T1-W2-H8
    • AWS A5.29; E81T1-W2C/W2M
    • ASME SFA 5.29

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Yield Strength 80 ksi, 550 MPa
Tensile Strength 90 ksi, 620 MPa
Reduction in Area 61.2 %
Elongation in 2" 24.0 %
As Welded CO2  
Yield Strength 79 ksi, 545 MPa
Tensile Strength 88 ksi, 605 MPa
Reduction in Area 61.0 %
Elongation in 2" 26.0 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded 75% Ar / 25% CO2 39 ft.-lbs., 53 J
As Welded CO2 34 ft.-lbs., 46 J
Testing Temperature -20ºF (-29ºC)  
As Welded 75% Ar / 25% CO2 34 ft.-lbs., 46 J
As Welded CO2 24 ft.-lbs., 33 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.044 %
Mn 1.01 %
Si 0.62 %
P .012 %
S .010 %
Cr .59 %
Ni 0.60 %
Cu 0.54 %
CO2  
C 0.047 %
Mn .74 %
Si 0.44 %
P .012 %
S .009 %
Cr .54 %
Ni 0.59 %
Cu .50 %

SAW

Accessories

Depositions

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.045 in, 1.2 mm 150 A A 28 200 ipm, 508 cm/min 4.2 lbs./hr., 1.91 kg./hr. 86 %
210 A A 29 300 ipm, 762 cm/min 6.3 lbs./hr., 2.86 kg./hr. 86 %
250 A A 30 400 ipm, 1016 cm/min 8.5 lbs./hr., 3.86 kg./hr. 87 %
290 A A 33 500 ipm, 1270 cm/min 10.7 lbs./hr., 4.85 kg./hr. 87 %
330 A A 34 600 ipm, 1524 cm/min 12.7 lbs./hr., 5.76 kg./hr. 87 %
.052 in, 1.4 mm 155 A A 25 150 ipm, 381 cm/min 4.4 lbs./hr., 2 kg./hr. 87 %
245 A A 28 250 ipm, 635 cm/min 7.3 lbs./hr., 3.31 kg./hr. 86 %
310 A A 33 350 ipm, 889 cm/min 10.2 lbs./hr., 4.63 kg./hr. 85 %
360 A A 36 450 ipm, 1143 cm/min 13.3 lbs./hr., 6.03 kg./hr. 85 %
430 A A 37 600 ipm, 1524 cm/min 17.6 lbs./hr., 7.98 kg./hr. 87 %
1/16 in, 1.6 mm 190 A A 27 150 ipm, 38 cm/min 6.1 lbs./hr., 2.77 kg./hr. 87 %
300 A A 30 250 ipm, 635 cm/min 10.2 lbs./hr., 4.63 kg./hr. 87 %

Extra Info

Shielding Gas

100% CO2 or Argon / CO2 mixtures