Designed for flat and horizontal position welding using CO2 shielding gas, Dual Shield 700X provides high deposition rates, high efficiency and excellent performance.
Dual Shield 710X is an all-position flux cored wire that offers outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.
Dual Shield 710X-M is an all-position flux cored wire for general purpose welding.
Dual Shield II 711X is an all-position flux cored wire that displays exceptional impact properties in combination with CO2 shielding gas.
Dual Shield II 712X is an all-position mixed gas flux cored wire intended for applications requiring outstanding weld metal toughness.
Dual Shield 810X-Ni1 is an all position 1% Nickel flux cored wire for general purpose welding.