Dual Shield 810X-Ni1 is an all position 1% Nickel flux cored wire for general purpose welding.
Dual Shield 810X-Ni1 provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 810X-Ni1 is designed for use with 100% CO2. It is an excellent choice for welding on COR-TEN® steel in applications where weathering grade wires are not desirable.

| As Welded | |
|---|---|
| Shielding Gas | CO2 |
| Yield Strength | 86 ksi, 590 MPa |
| Tensile Strength | 92 ksi, 635 MPa |
| Elongation (In 2", 51 mm) | 29 % |
| Typical Charpy V-Notch Impact Properties | |
| Shielding Gas | CO2 |
| Testing Temperature | |
| -20°F (-29°C) | 60 ft. - lbs., 81 J |
| -40°F (-40°C) | 45 ft. - lbs., 61 J |
| Typical Undiluted Weld Metal Analysis (%) | |
| Shielding Gas | CO2 |
| C | 0.04 |
| Mn | 1.3 |
| Si | 0.6 |
| P | 0.010 |
| S | 0.009 |
| Ni | 1.0 |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 245023023 | DS 810X-NI1 1/16X600# OMP | 662303087777 |
| 245022066 | DS 810X-NI1 1/16X50# CL | 662303085506 |
| 245022090 | DS 810X-NI1 1/16X60# CL | 662303085995 |
| 245022124 | DS 810X-NI1 052X25# AWS | 662303086657 |
| 245022132 | DS 810X-NI1 052X33# AWS | 662303086664 |
| 245022173 | DS 810X-NI1 1/16X600# RL | 662303087814 |
| 245022082 | DS 810X-ni1 1/16x33 #AWS | |
| 245022074 | DS 810X-Ni1 045x33 #AWS |
| Diameter | Amperage | Voltage | Wire Feed Speed | Deposition Rate | TTW |
|---|---|---|---|---|---|
| .045 in. | 115 A | 21.0 V | 160 ipm | 2.7 | 0.625 |
| 240 A | 27.5 V | 400 ipm | 10.5 | 0.625 | |
| .052 in. | 124 A | 21.0 V | 160 ipm | 3 | 0.75 |
CO2