Print this page

OK FLUX 350

OK Flux 350 is an active bonded flux for making butt and fillet welds in carbon steel plate up to 1" (25 mm) thick.

Ordering Information
SKU8291F09
UPC662303074777
Model / Product DescriptionOK FLUX 350 14X65 50#BG
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Weight50 lbs.
PackageBag