OK Flux 429 is a neutral, bonded flux intended for butt and fillet welding of carbon and low alloy steel plate.
| SKU | 8424F09H |
|---|---|
| UPC | 662303078737 |
| Model / Product Description | OK FLUX 429 14X65 55#BG |
| Item Weight | 55.00 |
| Min Order | 55 |
| Weight | 55 lbs. |
| Package | Bag |