OK Flux 350 is an active bonded flux for making butt and fillet welds in carbon steel plate up to 1" (25 mm) thick.
| SKU | 829AF09 |
|---|---|
| UPC | 662303076832 |
| Model / Product Description | OK FLUX 350 14X65 2200#BG |
| Item Weight | 2,200.00 |
| Min Order | 2200 |
| Filler Metal Spec Def | |
| Size | 14X65 |
| Weight | Bag lbs. |
| Package | Bag |