SUREWELD 10P Plus

Sureweld 10P-Plus is an all-position cellulosic electrode developed for the pipe welding industry. This electrode provides a more consistent burn-off and more forgiving arc burn when compared to Sureweld 10P. It produces X-ray quality joints in all-positions.

Ordering Information
SKU811004183
UPC662303050733
Model / Product DescriptionSW 10P PLUS 7/32X18X50#HS
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size7/32
Length18 in.
Weight50 lbs.
PackageHermetically Sealed Can