SUREWELD 810P

Sureweld 810P is an all-position cellulosic electrode developed for the pipe welding industry. This electrode is recommended for welding API pipe grades up to X70. It produces X-ray quality joints in all-positions and is noted for its deep, consistent penetration.

Ordering Information
SKU811070440
UPC662303070076
Model / Product DescriptionSW 810P 1/8X14X5#VALP
Item Weight5.00
Min Order5
Filler Metal Spec Def 
Size1/8
Length14 in.
Weight5 lbs.
PackageValue Pack