Sureweld 716P

Sureweld 716P contains a special lime coating which permits trouble-free welds on “difficult” steels such as high-carbon, alloy, high-sulfur, free-machining and cold-rolled steels. This pipe welding electrode is specially designed for pipe up to API 5LX65.