Sureweld SW-15 is an all-position electrode that can be used for a wide range of applications for light gauge and heavyplate. High heat and speeds can be used without undercut. The slag is easy to clean and even self-cleaning on heavy plate.
| SKU | 811061175 |
|---|---|
| UPC | 662303057497 |
| Model / Product Description | SW 15 3/32X12X10#VALP |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | 3/32 |
| Length | 12 in. |
| Weight | 10 lbs. |
| Package | Value Pack |