SUREWELD SW-15

Sureweld SW-15 is an all-position electrode that can be used for a wide range of applications for light gauge and heavyplate. High heat and speeds can be used without undercut. The slag is easy to clean and even self-cleaning on heavy plate.

Ordering Information
SKU811061183
UPC662303057565
Model / Product DescriptionSW 15 5/32X14X10#VALP
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size5/32
Length14 in.
Weight10 lbs.
PackageValue Pack

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.