SUREWELD 6013-LV

Sureweld 6013-LV is an all-position electrode designed to operate on low voltage AC power sources that have less than 50 open circuit volts. It is ideal for poor fit-up applications. This electrode can be used on thin gauge carbon and galvanized steels and is ideal for the hobby welder.

Ordering Information
SKU811061530
UPC662303019624
Model / Product DescriptionSW 6013LV 1/8X14X50#CT
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size1/8 , 14
Length14 in., 50 in.
Weight50 lbs., Carton lbs.
PackageCarton