SUREWELD 6013-LV

Sureweld 6013-LV is an all-position electrode designed to operate on low voltage AC power sources that have less than 50 open circuit volts. It is ideal for poor fit-up applications. This electrode can be used on thin gauge carbon and galvanized steels and is ideal for the hobby welder.

Ordering Information
SKU811062058
UPC662303064204
Model / Product DescriptionSW 6013LV 5/32X14X5#VALP
Item Weight5.00
Min Order5
Filler Metal Spec Def 
Size5/32 , 14
Length14 in., 5 in.
Weight5 lbs., Value Pack lbs.
PackageValue Pack