Print this page

SUREWELD SW-15 IP

Sureweld SW-15 IP is an all-position, iron powder coated electrode suitable for welding many types of mild steels in avariety of applications. It’s designed to permit the use of higher welding currents while improving deposition rate. High heats and speeds can be used without undercut, and the slag removal is excellent.

Ordering Information
SKU811041326
UPC662303057442
Model / Product DescriptionSW 15IP 5/32X14X5#VALP
Item Weight5.00
Min Order5
Filler Metal Spec Def 
Size5/32 , 14
Length14 in., 5 in.
Weight5 lbs., Value Pack lbs.
PackageValue Pack

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.