Atom Arc 7018-B2L is an all-position low hydrogen electrode with an extra low carbon analysis and a 1% Cr - 0.5% Mo weld metal analysis for reduced cracking. These are excellent for power piping, boiler work, castings and forgings.
| SKU | 255181497 |
|---|---|
| UPC | 662303080938 |
| Model / Product Description | AA 7018-B2L 5/32X14X10#HS XF |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | 5/32 |
| Length | 14 in. |
| Weight | 10 lbs. |
| Package | Hermetically Sealed Can |