ATOM ARC 8018-CM

Atom Arc 8018-CM is an all-position low hydrogen electrode used for welding steels such as 0.5% Cr - 0.5% Mo, 1% Cr -0.5% Mo, and 1% Cr - 0.5% Mo. Primarily used in power piping and boiler work for the fabrication of plates, pipes, tubes, castings and forging.

Ordering Information
SKU255051476
UPC662303081294
Model / Product DescriptionAA 8018-CM 3/32X12X40#HS XF
Item Weight40.00
Min Order40
Filler Metal Spec Def 
Size3/32
Length12 in.
Weight40 lbs.
PackageHermetically Sealed Can