ATOM ARC 8018-CM

Atom Arc 8018-CM is an all-position low hydrogen electrode used for welding steels such as 0.5% Cr - 0.5% Mo, 1% Cr -0.5% Mo, and 1% Cr - 0.5% Mo. Primarily used in power piping and boiler work for the fabrication of plates, pipes, tubes, castings and forging.